Standards / Q355B vs S355JR: What Buyers Should Know
③ 标准/对比页

Q355B vs S355JR: What Buyers Should Know

Q355B and S355JR look similar on paper - both nominal 355 MPa minimum yield. Here is how they actually differ, and when one can replace the other.

Two StandardsQ355B follows GB/T 1591 (China); S355JR follows EN 10025-2 (Europe). Both target 355 MPa minimum yield.
When to SubstituteCheck impact test temperature: S355JR requires +20 C Charpy; Q355B impact requirement depends on the quality suffix (B = +20 C). For most structural welding they are interchangeable with written approval.
Practical AdviceMatch by application and welding procedure, not by name alone - and confirm with mill certificates.
ItemQ355BS355JR
StandardGB/T 1591EN 10025-2
Yield>=355 MPa>=355 MPa
Impactby grade suffix+20 C
RegionChinaEurope
51product.online v1.9 · 2026-09-26